您好,歡迎訪問禹城泰瑞彩鋼復(fù)合板加工廠!

服務(wù)熱線

18765446878

熱門關(guān)鍵詞:禹城彩鋼廠,禹城彩鋼復(fù)合板,禹城鋼結(jié)構(gòu)板房 彩鋼板房
當(dāng)前位置:首頁>新聞資訊>新聞動態(tài)彩鋼板出現(xiàn)老化現(xiàn)象后要如何修復(fù)

彩鋼板出現(xiàn)老化現(xiàn)象后要如何修復(fù)

來源:http://www.fptdc.cn 日期:2022-11-14 發(fā)布人:
彩鋼板長期使用會老化。若老化嚴(yán)重,將影響鋼板的正常使用,帶來隱患。所以,使用時應(yīng)注意觀察電路板的使用情況。出現(xiàn)老化現(xiàn)象后可進(jìn)行修復(fù)。那裝修施工的具體步驟是什么呢?濟(jì)南彩鋼廠家為您解析。
Color steel plate will age after long-term use. If the aging is serious, it will affect the normal use of the steel plate and bring potential safety hazards. Therefore, the use of the circuit board should be observed. The aging phenomenon can be repaired. What are the specific steps of decoration construction? Jinan color steel manufacturers analyze for you.
1.彩鋼板底部的底板,并進(jìn)行除銹打磨。
1. Remove the bottom plate of the color steel plate, and conduct rust removal and polishing.
2.采用防腐專用底漆施工,對該夾芯板銹蝕特別嚴(yán)重的部位,應(yīng)采用重防腐底漆噴涂處理。
2. The special anti-corrosion primer shall be used for construction. The parts of the sandwich panel with severe corrosion shall be sprayed with heavy anti-corrosion primer.
3.由于彩鋼巖棉夾心板厚度為0.32mm,采用防腐專用面層噴涂二次。
3. As the thickness of color steel rock wool sandwich plate is 0.32mm, it is sprayed twice with a special anti-corrosion surface layer.
4.使用刷子涂或噴涂滾筒。
4. Brush or spray the roller.

濟(jì)南彩鋼

表面清理:
Surface cleaning:
1.脫漆:原有漆膜涂層老化、起鼓、剝皮、舊漆膜須用鏟刀將其刮靜。
1. Paint stripping: the original paint film coating is aged, bulged, peeled, and the old paint film must be scraped with a blade.
2.除銹:將已發(fā)生銹蝕的氧化皮及翹起、龜裂的部位用鏟刀、鋼絲刷、紗布和磨光機(jī)等工具打磨干凈,金屬表面應(yīng)達(dá)到無銹蝕、無油污、無雜物,并露出均一的金屬光澤,除銹等級達(dá)到St3 級標(biāo)準(zhǔn),同時除銹部位與保留的舊漆層邊緣須有平滑過度。
2. Derusting: The rusted oxide skin and the parts with warping and cracking shall be polished with shovel, wire brush, gauze, polishing machine and other tools. The metal surface shall be free of rust, oil stain and sundries, and the uniform metallic luster shall be exposed. The derusting grade shall meet the St3 standard. At the same time, the derusting part and the edge of the retained old paint layer must be smooth.
3.打磨和清洗:表面脫漆除銹后,須用砂輪或粗布對其打磨,磨出一定的粗糙度,增強(qiáng)油漆的附著力,然后進(jìn)行清洗,達(dá)到金屬表面無雜物、灰塵等。
3. Grinding and cleaning: After the surface is stripped of paint and derusted, it must be polished with a grinding wheel or rough cloth to obtain a certain roughness, enhance the adhesion of the paint, and then cleaned to ensure that the metal surface is free of debris, dust, etc.
4.對于有油漬的地方,需要先用清洗劑清理干凈。
4. Oil stains shall be cleaned with detergent first.
標(biāo)準(zhǔn):清理后,管道、罐體、支架、設(shè)備等防腐表層要求無浮塵、無浮銹、無層銹、無鼓包和翹皮的漆層、無砂漿疙瘩、無油漬和化學(xué)腐蝕物。 作者:代諾重防腐防銹涂料 https://www.bilibili.com/read/cv11986023/ 出處:bilibili
Standard: After cleaning, the anti-corrosion surface of pipes, tanks, supports, equipment, etc. shall be free of floating dust, floating rust, layer rust, bulged and warped paint, mortar bumps, oil stains and chemical corrosives. Author: Danuo Heavy Anti corrosion and Anti rust Paint https://www.bilibili.com/read/cv11986023/ Origin: bilibili
彩鋼板的翻新過程還是比較簡單的,在翻新時要注意把底板的底面打磨干凈,把生銹的地方磨平,接著進(jìn)行涂料噴刷,記得要噴刷均勻,這樣才能保證表面牢固度不容易脫落,相信大家掌握以上方法后可以很好的進(jìn)行翻新工作。更多相關(guān)內(nèi)容就來我們網(wǎng)站http://www.fptdc.cn咨詢看看吧!
The renovation process of color steel plate is relatively simple. During the renovation, the bottom surface of the base plate should be polished clean, the rusty area should be smoothed, and then the paint should be sprayed evenly, so as to ensure that the surface firmness is not easy to fall off. I believe that you can carry out the renovation work well after mastering the above methods. Come to our website for more http://www.fptdc.cn   information!